Journal of the Society of Motion Picture and Television Engineers ( Volume: 57, Issue: 2, August 1951)
[ACTIVE]
Modified Negative Perforation: Proposed as a Single Standard for 35-mm Negative and Positive Motion Picture Film
Metadata
- Publisher
- SMPTE — White Plains, NY, USA
- Doc Type
- Journal Article
- Content Type
- Original Research
- Abbreviated Title
- J SMPTE
- Volume
- 57, No. 2, pp. 108–123
- Abstract
- The existence of two or more perforation shapes for 35-mm films has, for many years, been considered undesirable. For processes requiring accurate film positioning, the dual Standard of Negative perforation for camera stock and Positive perforation for release stock does not suffice. Registration problems are minimized if Negative perforations are used throughout; experience, however, has shown that projection life is short. The Modified Negative perforation, with fillets at the corners, has improved resistance to tear while preserving the general negative form corresponding to conventional piloting means. Tests conducted show that better film positioning is accomplished in conventional camera and printing equipment for film with Modified Negative perforations than for film with Dubray-Howell perforations. The method of evaluating film location during exposure and printing is described and evidence of results presented. Photoelectrically recorded charts show the extent of out-of-register which resulted for various combinations of perforation types. Film-life projection tests indicate that the Modified Negative perforation is equal or superior to the Dubray-Howell perforation.
- Publication Date
- 1951-08-01
- DOI
10.5594/J05054- ISSN
- Print:
0898-042X - Link
- https://doi.org/10.5594/J05054
- Author(s)
- W. G. HillAnsco Division, General Aniline & Film Corp., Binghamton, N.Y.
- Copyright
- © 1951 Society of Motion Picture and Television Engineers, Inc.
Bibliographic Reference(s)
- 1. Proposed American Standard , Jour. SMPE , vol. 52 , pp. 447 – 452 , Apr. 1949 . EXTERNAL
- 2. Report of the Subcommittee on Perforation Standards . Jour. SMPE , vol. 29 , pp. 376 – 387 , Oct. 1937 . EXTERNAL
Source Data (JSON)
Full registry record with provenance metadata. Open directly: /api/doc/10.5594-J05054.json
Reference Tree
Explore all references and references to this document, as a navigable tree.
Open Reference TreeReference this Doc
Plain text (ISO 690 compliant)
Preview:
W. G. Hill; Modified Negative Perforation: Proposed as a Single Standard for 35-mm Negative and Positive Motion Picture Film, Journal of the Society of Motion Picture and Television Engineers ( Volume: 57, Issue: 2, August 1951); SMPTE, 1951. Available at https://doi.org/10.5594/J05054
Snippet:
W. G. Hill; Modified Negative Perforation: Proposed as a Single Standard for 35-mm Negative and Positive Motion Picture Film, Journal of the Society of Motion Picture and Television Engineers ( Volume: 57, Issue: 2, August 1951); SMPTE, 1951. Available at https://doi.org/10.5594/J05054
HTML (ISO 690 compliant)
Preview:
W. G. Hill; Modified Negative Perforation: Proposed as a Single Standard for 35-mm Negative and Positive Motion Picture Film, Journal of the Society of Motion Picture and Television Engineers ( Volume: 57, Issue: 2, August 1951); SMPTE, 1951. Available at https://doi.org/10.5594/J05054
Snippet:
<span class="citation">W. G. Hill; <cite>Modified Negative Perforation: Proposed as a Single Standard for 35-mm Negative and Positive Motion Picture Film</cite>, Journal of the Society of Motion Picture and Television Engineers ( Volume: 57, Issue: 2, August 1951); SMPTE, 1951. Available at <a href="https://doi.org/10.5594/J05054" target="_blank" rel="noopener">https://doi.org/10.5594/J05054</a></span>
SMPTE's HTML Pub
Preview:
W. G. Hill; Modified Negative Perforation: Proposed as a Single Standard for 35-mm Negative and Positive Motion Picture Film, Journal of the Society of Motion Picture and Television Engineers ( Volume: 57, Issue: 2, August 1951); SMPTE, 1951
doi: 10.5594/J05054
url: https://doi.org/10.5594/J05054
doi: 10.5594/J05054
url: https://doi.org/10.5594/J05054
Snippet:
<li> W. G. Hill; <cite id="bib-10-5594-j05054">Modified Negative Perforation: Proposed as a Single Standard for 35-mm Negative and Positive Motion Picture Film</cite>, Journal of the Society of Motion Picture and Television Engineers ( Volume: 57, Issue: 2, August 1951); SMPTE, 1951 <span class="doi">10.5594/J05054</span> </li>
Referenced By
- “Managing” the Moving Image — From an Engineering Point of View [Active]
- “Managing” the Moving Image—From an Engineering Point of View—Part II [Active]
- “Managing” the Moving Image—From an Engineering Point of View—Part I [Active]
- A Tutorial Paper: Motion-Picture Film — Its Size and Dimensional Characteristics [Active]
- A Method of Measuring the Steadiness of Motion-Picture Cameras [Active]