Abstract
The 4:2:2 component recording system (Type D-1) records signals at a rate of over 200 Mb/sec with a shortest recording wavelength of only 0.9 um. Low error rates (in the order of 10–6 to 10–7) can be obtained if a tape formulation can be developed with a high output and low noise characteristics optimized to record at these wavelengths. As the D–1 DVTR can only use ferrite video heads, a high coercivity cobalt oxide tape was developed to meet the needs of the format. The paper discusses why such a formulation was chosen and contrasts how the D–1 tape performs against other media when evaluated for the 4:2:2 standard.
Publication Date
1988-01-01
DOI
10.5594/M00524
Link
https://doi.org/10.5594/M00524
Author(s)
K. IsesakaSony Magnetics Products Inc. Japan
Y. FujimakiSony Magnetics Products Inc. Japan
T. NakamuraSony Magnetics Products Inc. Japan
S. TakahashiSony Magnetics Products Inc. Japan
K. KobyashiSony Corp. of America Park Ridge, New Jersey
S. Leader
Copyright
© 1988 Society of Motion Picture and Television Engineers, Inc.
Source Data (JSON)

Full registry record with provenance metadata. Open directly: /api/doc/10.5594-M00524.json

Reference this Doc

Plain text (ISO 690 compliant)

Preview:
K. Isesaka, Y. Fujimaki, T. Nakamura, S. Takahashi, K. Kobyashi, and S. Leader; The Application of High Hc Cobalt-Iron Oxide Tape for Digital Video Recording, SMPTE Meetings and Conferences ( January 1988); SMPTE, 1988. Available at https://doi.org/10.5594/M00524
Snippet:
K. Isesaka, Y. Fujimaki, T. Nakamura, S. Takahashi, K. Kobyashi, and S. Leader; The Application of High Hc Cobalt-Iron Oxide Tape for Digital Video Recording, SMPTE Meetings and Conferences ( January 1988); SMPTE, 1988. Available at https://doi.org/10.5594/M00524

HTML (ISO 690 compliant)

Preview:
K. Isesaka, Y. Fujimaki, T. Nakamura, S. Takahashi, K. Kobyashi, and S. Leader; The Application of High Hc Cobalt-Iron Oxide Tape for Digital Video Recording, SMPTE Meetings and Conferences ( January 1988); SMPTE, 1988. Available at https://doi.org/10.5594/M00524
Snippet:
<span class="citation">K. Isesaka, Y. Fujimaki, T. Nakamura, S. Takahashi, K. Kobyashi, and S. Leader; <cite>The Application of High Hc Cobalt-Iron Oxide Tape for Digital Video Recording</cite>, SMPTE Meetings and Conferences ( January 1988); SMPTE, 1988. Available at <a href="https://doi.org/10.5594/M00524" target="_blank" rel="noopener">https://doi.org/10.5594/M00524</a></span>

SMPTE Icon SMPTE's HTML Pub

Preview:
K. Isesaka, Y. Fujimaki, T. Nakamura, S. Takahashi, K. Kobyashi, and S. Leader; The Application of High Hc Cobalt-Iron Oxide Tape for Digital Video Recording, SMPTE Meetings and Conferences ( January 1988); SMPTE, 1988
doi: 10.5594/M00524
url: https://doi.org/10.5594/M00524
Snippet:
<li>
K. Isesaka, Y. Fujimaki, T. Nakamura, S. Takahashi, K. Kobyashi, and S. Leader; <cite id="bib-10-5594-m00524">The Application of High Hc Cobalt-Iron Oxide Tape for Digital Video Recording</cite>, SMPTE Meetings and Conferences ( January 1988); SMPTE, 1988
<span class="doi">10.5594/M00524</span>
</li>