- Abstract
- When 35mm color negative films are used repeatedly for release printing, they may become badly scratched. These scratched negatives give 16mm release prints of inferior quality in an optical reduction printing operation. The effects of scratches on the negative can be eliminated by applying a thin layer of liquid to the support side of the film just before printing. A Depue optical printer was modified by adding a roller applicator and liquid reservoir and by using an undercut pressure pad at the gate. This method is simpler and less expensive than liquid immersion printing and produces prints of high quality.
- Publication Date
- 1959-06-01
- DOI
10.5594/J13836- ISSN
- Print:
0361-4573 - Link
- https://doi.org/10.5594/J13836
- Author(s)
- Raymond H. DeMoulinEastman Kodak Co., Color Technology Div., Kodak Park Works, Rochester 4, N.Y.Philip A. RipsonEastman Kodak Co., Color Technology Div., Kodak Park Works, Rochester 4, N.Y.Stanley L. ScudderEastman Kodak Co., Color Technology Div., Kodak Park Works, Rochester 4, N.Y.
- Copyright
- © 1959 Society of Motion Picture and Television Engineers, Inc.
Bibliographic Reference(s)
- Printing Motion-Picture Films Immersed in a Liquid Part III: Evaluation of Liquids [Active]
- Printing Motion-Picture Films Immersed in a Liquid: Part I: Contact Printing [Active]
- Part II: Optical Printing [Active]
- 4. Quarterly Report on Current Prices. Chemical and Engineering News , Dec. 29, 1958 . EXTERNAL
Source Data (JSON)
Full registry record with provenance metadata. Open directly: /api/doc/10.5594-J13836.json
Reference Tree
Explore all references and references to this document, as a navigable tree.
Open Reference TreeReference this Doc
Plain text (ISO 690 compliant)
Preview:
Raymond H. DeMoulin, Philip A. Ripson, and Stanley L. Scudder; Application of a Liquid Layer on Negative Films to Eliminate Surface Defects in Optical Printing, Journal of the SMPTE ( Volume: 68, Issue: 6, June 1959); SMPTE, 1959. Available at https://doi.org/10.5594/J13836
Snippet:
Raymond H. DeMoulin, Philip A. Ripson, and Stanley L. Scudder; Application of a Liquid Layer on Negative Films to Eliminate Surface Defects in Optical Printing, Journal of the SMPTE ( Volume: 68, Issue: 6, June 1959); SMPTE, 1959. Available at https://doi.org/10.5594/J13836
HTML (ISO 690 compliant)
Preview:
Raymond H. DeMoulin, Philip A. Ripson, and Stanley L. Scudder; Application of a Liquid Layer on Negative Films to Eliminate Surface Defects in Optical Printing, Journal of the SMPTE ( Volume: 68, Issue: 6, June 1959); SMPTE, 1959. Available at https://doi.org/10.5594/J13836
Snippet:
<span class="citation">Raymond H. DeMoulin, Philip A. Ripson, and Stanley L. Scudder; <cite>Application of a Liquid Layer on Negative Films to Eliminate Surface Defects in Optical Printing</cite>, Journal of the SMPTE ( Volume: 68, Issue: 6, June 1959); SMPTE, 1959. Available at <a href="https://doi.org/10.5594/J13836" target="_blank" rel="noopener">https://doi.org/10.5594/J13836</a></span>
SMPTE's HTML Pub
Preview:
Raymond H. DeMoulin, Philip A. Ripson, and Stanley L. Scudder; Application of a Liquid Layer on Negative Films to Eliminate Surface Defects in Optical Printing, Journal of the SMPTE ( Volume: 68, Issue: 6, June 1959); SMPTE, 1959
doi: 10.5594/J13836
url: https://doi.org/10.5594/J13836
doi: 10.5594/J13836
url: https://doi.org/10.5594/J13836
Snippet:
<li> Raymond H. DeMoulin, Philip A. Ripson, and Stanley L. Scudder; <cite id="bib-10-5594-j13836">Application of a Liquid Layer on Negative Films to Eliminate Surface Defects in Optical Printing</cite>, Journal of the SMPTE ( Volume: 68, Issue: 6, June 1959); SMPTE, 1959 <span class="doi">10.5594/J13836</span> </li>